Aluminum welding wire (E4047)

Aluminum welding wire (E4047)
Product Detailed
Related Categories:Electric Hammer

Detailed Product Description


 

                                       Aluminum welding alloy 

Aluminum Welding wire  Specialized in production pure aluminum welding rod, aluminum magnesium welding rod, aluminum silicon welding rod, low silicon welding rod, high silicon welding rod.

The product surface is luminous, and the welding performance is good. It is used in each kind of aluminum material welding.

Technology data for your reference:

AWS

Joint Strength

 Parent metal

Characteristics

Standard

(Mpa)

ER1070

Above 55

Pure aluminum series105010701080

Good anti-corrosive and plasticity

ER1100

80-110

Pure aluminum  series1100

Good anti-corrosive and plasticity

ER1200

80-110

Pure aluminum  series1200

Good anti-corrosive and plasticity

ER2319

400-450

Pure aluminum  series2219

High intensity after heat treatment

ER4043

170-250

Al-Mg-Si casting aluminum

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER4047

170-250

Casting Al. ,Al-Cu casting ,Ag-Mg-Si casting

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER4145

200-300

Al-Cucasting20142017

The anti-thermal crack performance of the welded joint is good, but the plasticity, toughness are low, becomes grey black after anodic process

ER5554

180-240

low Mg content5052,5454casting

 Use chemical equipment with a temperature above 65

ER5654

210-270

medium Mg content5154casting

medium intensity,good anti-corrosive

ER5356

270-310

Al-Mg casting, Al-Mg-Si casting, Al-Zn-Mg casting

Typical welding wire used most widely, good mechanics performance and anti-corrosiveness

ER5556

280-320

Al-Zn-Mg casting, Al-Mg casting

The connector intensity is high, and the moulding performance and tenacity is inferior to 5183

ER5183

280-310

Al-Mgcasting5083

Typical welding wire used most widely, good mechanical performance and anti-corrosiveness